| 03/18/2016 || Thermal annealing || Ramp up at 18oC/hour up to 200oC. Stays for 10 hours and ramp down at 18oC/hour.
 
| 03/18/2016 || Thermal annealing || Ramp up at 18oC/hour up to 200oC. Stays for 10 hours and ramp down at 18oC/hour.
 +
|-
 +
| 04/13/2016 || Light Yield || Run 3171: crystal wrapped with ~5 layers of teflon tape and 2 layers of black tape. Steps of 20min, 1cm. T=18oC. LY = 14.95 pe/MeV.
 
|}
 
|}
  

Revision as of 23:45, 23 April 2016

⇐ Back to Crystal LOG
⇐ Back to Neutral Particle Spectrometer
⇐ Back to the Main_Page

Time LOG

SICCA J30
Date Description Comments
03/09/2016 Pictures Documentation of crystal's conditions as it arrived at CUA.
03/09/2016 Dimensions Crystal's dimensions measured. Length and six points of width (3 in each face).
03/18/2016 Thermal annealing Ramp up at 18oC/hour up to 200oC. Stays for 10 hours and ramp down at 18oC/hour.
04/13/2016 Light Yield Run 3171: crystal wrapped with ~5 layers of teflon tape and 2 layers of black tape. Steps of 20min, 1cm. T=18oC. LY = 14.95 pe/MeV.

Pictures at 03/09/2016

Stain shown on surface of crystal on one end.